Man, I tried to use some JB weld for the first time on those holes. It turned out to be a nightmare. That stuff is freaking difficult to work with. I put some in only two of the holes at first and it took forever to set, and I had to keep scooping it back into the holes as it oozed out. Then I took what was left in the tubes and mixed them and placed them under a little lamp I have. I check on the stuff under the lamp after less than an hour, and it was already too hard to use, meanwhile the stuff in my manifold is still goopy.(pissed)
Doh, I should have used quicksteel like in the How-To. I saw some stuff at the store that looked the same as quick steel, called fast steel or something, but it bothered me that it did not specify heat tolerances, so I didn't get it. I am a moron.
Doh, I should have used quicksteel like in the How-To. I saw some stuff at the store that looked the same as quick steel, called fast steel or something, but it bothered me that it did not specify heat tolerances, so I didn't get it. I am a moron.
Last edited: